RLM 257/125
low melting alloy 125 degree Centigrade
Melting point: 257 degrees F / 125 degrees Celsius
Includes: Bismuth and Lead
Shape: Ingots, Cakes, Bars
Bullion: 950–950 g
Cake: 500–450 g
Rod: 80-70 g
Includes: Bismuth and Lead
Shape: Ingots, Cakes, Bars
Bullion: 950–950 g
Cake: 500–450 g
Rod: 80-70 g
Safe Load Sustained - Bar* | Maximum Load-5 Minutes - Bar* | Maximum Load-30 Seconds - Bar* | Conductivity/Electrical Compared with Pure Copper | Latent Heat - Fusion - KJ/Kg* | Specific Heat - Solid* | Specific Heat - Liquid* | Brinell Hardness No. | Elongation in slow Loading % | Tensile Strength - Bar | Yield Temp - ° C | Melting Temperature - ° C | Properties |
20 | 276 | 550 | 3% | 16.7 | 0.030 | 0.042 | 10.2 | 60-70 | 441 | 125±3 | 125 | RLM 257/125 |
*Approximate
RLM |
- |
X/Y |
- |
I |
- |
Q |
1 |
|
2 |
|
3 |
|
4 |
|
|