70 ° C

RLM 158/70

low melting alloy 70 degree Centigrade

Melting point: 158 degrees F / 70 degrees Celsius

Includes: Bismuth, Lead, Tin, and Cadmium
Shape: Ingots, Cakes, Bars

Bullion: 950–950 g

Cake: 500–450 g

Rod: 80-70 g

Safe Load Sustained - Bar* Maximum Load-5 Minutes - Bar* Maximum Load-30 Seconds - Bar* Conductivity/Electrical Compared with Pure Copper Latent Heat - Fusion - KJ/Kg* Specific Heat - Solid* Specific Heat - Liquid* Brinell Hardness No. Elongation in slow Loading % Tensile Strength - Bar Yield Temp - ° C Melting Temperature - ° C Properties
20 276 690 4% 33 0.040 0.040 9.2 200 413 70±3 70 RLM 158/70

*Approximate

RLM

-

X/Y

-

I

-

Q

1

2

3

4

1- RLM:RATA Low Melting Point Alloys
2- Melting Temperature
X: 158, 203, 232, 257, 284, 320, 362 (Fahrenheit)
Y: 70, 95, 110, 125, 140, 160, 183 (Celsius)
* Melting Temp for Other Response Temperatures
3- Forms
I: Ingot
C: Cake
B: Bar
4- Quantity
Q: Quantity
* Min Order (15 Kg)